| property |
test method |
unit |
value |
phisical data
|
| thickness |
- |
micron |
24 (12/12) |
| coefficient of friction |
film/film |
ASTM-D-1894 |
- |
0,25-0,35 |
| yield2 |
|
m2/kg |
45,9 |
| treatment printable side1 |
- |
- |
CORONA |
| wettability printable side |
ASTM-D-2578 |
dyne/cm |
38 |
mechanical data
|
| tensile strenght |
MD |
ASTM-D-882 |
kg/cm2 |
630 |
| TD |
ASTM-D-882 |
kg/cm2 |
1500 |
| elongation at break |
MD |
ASTM-D-882 |
% |
165 |
| TDr |
ASTM-D-882 |
% |
50 |
thermal data
|
shrinkage (120 °C,
5 Min.)
|
MD |
ASTM-D-1204 |
% |
3,5 |
| TD |
ASTM-D-1204 |
% |
2,0-2,5 |
| lamination temperature3 |
- |
°C |
90 - 130 |
optical data
|
| gloss (45°) |
ASTM-D-2457 |
Gardner |
90 |
standard slitted rolls
|
| core |
- |
mm |
76 |
| length |
- |
m/roll |
3.000 |
| side with adhesive |
- |
- |
inside |
| glossy side |
- |
- |
outside |
| printable side1 |
- |
- |
outside |
The data contained here is provided according to the
best knowledge and is based on our general experience and tests undertaken
in our laminating film laboratories. But we cannot guarantee these data
in respect of factors, which are out of our control and responsibility.
Therefore compliance with all legal patents, copyrights, trademarks and
registered designs is responsibility of user.